SPECIFICATION : JIS G 3507
Grade No | Chemical Composition (%) | |||||
---|---|---|---|---|---|---|
C | Si | Mn | P | S | AL | |
SWRCH 8R | 0.10 Max | – | 0.60 Max | 0.040 Max | 0.040 Max | – |
SWRCH 6A | 0.08 Max | 0.10 Max | 0.030 Max | 0.035 Max | 0.020 Min | |
SWRCH 8A | 0.10 Max | |||||
SWRCH 18A | 0.15-0.20 | 0.60-0.90 | ||||
SWRCH 22A | 0.18-0.23 | 0.70-1.00 | ||||
SWRCH 35K | 0.32-0.38 | 0.10-0.35 | 0.60-0.90 | – | ||
SWRCH 38K | 0.35-0.41 | |||||
SWRCH 40K | 0.37-0.43 |